How to draft an AWS D1.1:2025 Welding Procedure Specification for Gas Metal Arc Welding (GMAW) on ASTM A36 Carbon Structural Steel. Recommended filler: ER70S-6. Below: process notes, base metal properties, prequalification path, typical parameters, and which essential variables to watch.
About GMAW (Gas Metal Arc Welding)
Solid-wire continuous-feed process with external shielding gas (typically 75/25 Ar/CO₂ or 90/10 Ar/CO₂). Constant voltage (CV) output and a fixed wire feed speed give a stable arc. Transfer mode (short-circuit, globular, spray, pulsed) is selected by voltage + current combination. Note: A5.36 was dropped from the AWS D1.1:2025 Table 6.6 allowed-spec list for GMAW.
Process family: semi-auto. Suited to: shop fabrication of structural members, high-deposition shop welds, and similar work.
About ASTM A36
The default structural carbon steel for non-critical applications. Carbon content typically 0.25-0.29%, low carbon equivalent, excellent weldability with both low-hydrogen and non-low-hydrogen consumables. Plate, bar, and shapes.
- AWS D1.1:2025 Group (Table 5.6)
- Group I to 3/4 in, II above
- Yield (ksi)
- 36
- Tensile (ksi)
- 58–80
- Weldability
- excellent
Prequalification path
ASTM A36 (Group I to 3/4 in, II above) is on the prequalified base metals list for GMAW per AWS D1.1:2025 Clause 5. A written WPS is still mandatory but no PQR test is required as long as every Clause 5 essential variable (joint geometry, filler, preheat, current/polarity, etc.) is met.
Preheat: No preheat required for thicknesses ≤ 3/4 in at typical heat inputs; 50°F minimum below 3/4 in, 150°F at 1-1/2 in and above per Table 5.7.
Typical parameters
Starting points only. Verify against electrode manufacturer data and your PQR.
| Filler | ER70S-6 |
| Amperage | 150–280 A (0.045 in wire) |
| Voltage | 22–28 V (spray transfer) |
| Travel speed | 10–25 ipm |
| Position(s) typically qualified | All positions (1G–4G); 5G/6G for pipe per Clause 10 |
Essential variables to watch (AWS D1.1:2025 Table 6.6)
If your shop is working from a PQR, these are the GMAW-specific changes that require requalification per Table 6.6. The rule engine flags every one of them with the row number, clause reference, and the actual delta.
- Shielding gas composition (any change)
- Voltage > 7% change
- Amperage > 10% change
- Wire diameter increase
- Transfer mode change (short-circuit ↔ spray ↔ pulsed)
- CV ↔ CC output change
Where GMAW on ASTM A36 fits
- Light to medium structural framing
- Miscellaneous and ornamental steel
- Base plates and gussets
- Non-load-critical components
Start now
Draft this WPS in the next 2 minutes.
Create a free account and the editor opens with this GMAW + ASTM A36 setup preselected. Free drafts are rules-checked; the 14-day trial adds AI narrative with inline AWS D1.1:2025 citations. Export as a PDF, your CWI signs.
Related WPS templates
FAQ
Does AWS D1.1:2025 prequalify GMAW on ASTM A36?
Yes — ASTM A36 is on the Clause 5 prequalified base metals list and GMAW is a Clause 5 prequalified process. You still need a written WPS but no PQR.
What filler is recommended for GMAW on ASTM A36?
ER70S-6. Verify against your project specification and the consumable manufacturer's data sheet. Filler classification change is a Table 6.6 essential variable.
What preheat does ASTM A36 need?
No preheat required for thicknesses ≤ 3/4 in at typical heat inputs; 50°F minimum below 3/4 in, 150°F at 1-1/2 in and above per Table 5.7.